Product physical properties:
Melting degree: 220°C
Specification: 0.11~1.5 (mm)
Fracture strength range: 6.7~7.1 (N)
Fracture elongation range: 20.6~23.1 (%)
Boiling water shrinkage range: 7.9~10.3 (cm)
Dry heat shrinkage range: 12~13.9 (cm)
Applications of Two Component Hot Melt Monofilament Yarn
Nonwoven & Technical Textiles: Used in hygiene products, filters, and geotextiles for layer bonding.
Automotive Interiors: Bonds fabric layers in headliners, door panels, and trunk linings.
Footwear & Apparel: Provides seamless bonding in shoe components and garment reinforcements.
Furniture & Mattresses: Laminates fabric layers in upholstery and padding.
As a specialized two component hot melt monofilament supplier, BOSIDI offers advanced monofilament solutions designed for thermal bonding applications. Two component hot melt monofilament is a core-sheath structured filament where the outer sheath has a lower melting point than the inner core. When heated, the sheath melts to create strong adhesive bonds between materials while the core maintains structural integrity. This innovative product enables efficient, binder-free joining of fabrics and nonwovens.